1.Molding machine can not stick
Heating temperature is too high or too low, forming sets of serious wear and tear, propulsion point of view does not match the raw water is too large. Forming Machine Forming normal working hours in rods from the sleeve uniform extrusion, bar should be dark brown, uniform hardness, surface smoothness no cracks, the center hole of the surface is also smooth, smooth exhaust.


2.Bright surface
Cross-section of the rod has a light, density, though good but the hardness of the poor. This is the first Road Department spiral initial reasons too steep, it should be smooth some polishes.


3.Surface crack
Raw water is too large rod body easily produce transverse crack, water is too small, while leading to the emergence of vertical cracks. In addition, the heating temperature is too high cause excessive softening of raw materials, which led to lack of feed.

This would also lead to the emergence of crack. General solution for the shortage of materials is appropriate to increase the diameter of spiral or helical wall polished to increase the profile distance between spiral.


4.The center rod density, or contains scattered sawdust
This is because the propeller shaft diameter of the root tip wear, it is necessary to repair welding bold. Shaft tip errors can also lead to the above problems, to be under high temperature and its correction.


5.Anti-gas.
Manifested in the production of materials from the mouth outward emitted gases, mainly due to lack of feed. Raw materials may also be due to excessive moisture, inadequate heating temperature.


 

China Briquetting Press Machine, Briquette Machines for Sale
CopyRight © 2000-2008 briquette-machine.com- All Rights Reserved.tag
Tel: 0086 372 5951936 Fax: 0086 372 5951936 E-mail: sales@agico.com.cn

Sawdust Briquetting Presses